Fresa plana PDC
Oil, water well and coal drilling; primary or gauge positions
- Aplicación / ajusteOil, water well and coal drilling; primary or gauge positions
- Diámetro8.00–19.05 mm (0.315–0.750 in) de diámetro
- MaterialPCD diamond table on tungsten carbide
- MountingBit pocket brazing; pocket diameter follows selected OGF size