PRODUCTDESIGN
The innovative Step-shaped PDC cutter design revolutionizes cutter replacement with its bolt fixation system, abandoning traditional brazing methods. This forward-thinking approach enables swift and seamless swaps of worn-out cutters with new ones, significantly boosting operational efficiency. The cleverly engineered small steps at the bottom of these cutters provide a secure anchor point, allowing for robust bolt fastening to the equipment.
This clever design tweak translates to reduced downtime, minimized labor costs, and increased productivity. By simplifying the replacement process, operators can quickly get back to drilling, ensuring uninterrupted progress and maximizing their drilling potential.

Excellent Wear Resistance
Using a polycrystalline diamond layer, Flat PDC Cutters have extremely high hardness.

Customized Services
Customized according to specific needs, including shape, wear resistance, impact resistance, etc.

Preeminent Thermal Stability
It is not easy to deform or fail due to thermal expansion, thus ensuring the continuity and safety of drilling operations.

Outstanding Impact Resistance
With strong shock and vibration, thereby extending the service life.
PRODUCTSPECIFICATIONS
| Type | Diameter | Height | Diamond layer height | Step height | Step diameter | Diamond chamfer size |
| SCS0808 | 8.00mm | 8.00mm | 2.0mm | 1.5mm | 4mm | 0.40mm×45° |
| SCS1008 | 10.00mm | 8.00mm | 2.0mm | 1.5mm | 4mm | 0.40mm×45° |
| SCS1308 | 13.44mm | 8.00mm | 2.0mm | 1.5mm | 6mm | 0.40mm×45° |
| SCS1311 | 13.44mm | 11.00mm | 2.0mm | 3mm | 6mm | 0.40mm×45° |
| SCS1313 | 13.44mm | 13.20mm | 2.0mm | 5.2mm | 6mm | 0.40mm×45° |
OURADVANTAGES
These distinct advantages can significantly aid Field Diamond in distinguishing itself amidst the fiercely competitive market landscape, effectively bolstering its overall competitiveness and positioning it as a leading player in its industry.
- Leading Technology Innovation
- High Production Efficiency
- Optimized Cost Control
- Strict Quality Control
- Green and Environmentally Friendly Production
16K+
Customer
Satisfied
500+
Campaigns
98%
Client Satisfaction
7+
Years Experiences
15+
Certified Experts
APPLICATIONAREAS
Natural gas & Oiloperation ——
Down-the-hole hammer ——
Water well building ——
Geological
exploration ——
• All Projects
With the strength and impact resistance of cemented carbide, it is an ideal material for manufacturing wear-resistant tools such as cutting tools and drills, and has a wide range of applications in oil drilling, geological exploration, coal mine drills, mechanical processing tools and other industries.
With its exceptional strength and impact resistance, cemented carbide is an ideal material for manufacturing wear-resistant tools, widely applied in oil drilling, geological exploration, mining, machinery, and more.
PRODUCTIONPROCESS
The process begins with the preparation of raw materials, which are screened and inspected to ensure their quality meets production requirements. The raw material then enters the HTHP (high temperature and high pressure) synthesis stage, where it is converted into synthetic blocks through specific process conditions.
Next, the synthetic block goes through a series of treatment steps, including machining, grinding, etc., to further improve its properties and shape. In this process, advanced technologies such as electric discharge machining (EDM) and shaping are also used to ensure the accuracy and surface quality of the product.
Finally, after fine processing such as laser treatment, the individual parts are assembled together to form the final product. The entire production process is rigorous and efficient, reflecting the advanced nature and professionalism of modern production.
FACTORYSHOWCASE
Field Diamond help companies stand out in the fierce market competition.
Our factory integrates advanced equipment, exquisite technology and efficient management, and ensures excellent product quality with strict quality control system. We have a professional research and development team, continuous innovation, to meet the needs of diversified markets. Large-scale production to reduce costs, to provide cost-effective quality products, to win customer trust and praise.
325+
Complete Projects
15+
Certified Experts
750+
Innovative Solutions Deployed
1000+
Milestones Achieved in Development
Scale production
Advanced equipment, production processes.
High-effect
High degree of equipment automation, excellent product quality and stability.
Lean manufacturing
Intelligent and efficient equipment, streamlined and smooth process.
SOMEFAQ
● PDC Cutter FAQ
PDC composite sheet is a composite material sintered by diamond micropowder and cemented carbide substrate under ultra-high pressure and high temperature conditions, which combines the high hardness and wear resistance of diamond and the strength and impact toughness of cemented carbide.
UsualPDC tools are widely used in oil drilling, geological exploration, mechanical processing, wood processing and other fields.
PDC tools have higher hardness, wear resistance and thermal stability, which can significantly improve the durability and processing quality of the tool, and have better economy.
The PDC composite sheet is made of natural or synthetic diamond powder and binder (including cobalt, nickel and other metals) sintered on the cemented carbide matrix at high temperature and pressure.
● Custom service and technical support FAQ
Yes, we offer customized services for PDC tools to meet the specific needs of different customers.
The delivery time for customized products depends on the specific customization content and production schedule. Generally, after receiving the customization request, we will assess it as soon as possible and provide an estimated delivery time.
We offer comprehensive technical support, including product selection consultation, installation guidance, troubleshooting, and resolution. Customers can contact us via phone, email, or online chat tools to obtain timely technical support.
● Production and processing of PDC tools FAQ
Our production process includes raw material preparation, mixing, sintering, grinding and polishing and other links, each link has undergone strict quality control to ensure stable and reliable product performance.
We use advanced production equipment and technology, high production efficiency, can meet the needs of large orders.
The processing process of PDC tool includes the cutting of PDC composite sheet, blade welding, blade sharpening and other steps, each link needs precise control to ensure tool performance.
We use advanced processing equipment and technology, while equipped with professional technical personnel for quality control, to ensure that the processing accuracy of PDC tools meet customer requirements.
● Order FAQ
You can order online through our official website, or you can contact our sales team directly for product information and help. For large purchases or customized needs, it is recommended to communicate in detail by email or phone, so that we can provide you with more accurate quotes and services.
Generally, standard products are shipped within 3-7 working days after order confirmation and payment. For customized or specially configured products, the shipping time may be slightly longer, subject to our production schedule and customer communication. We will notify you of the estimated shipping date in advance.
We support multiple payment methods, including but not limited to bank transfers, credit card payments (through third-party payment platforms), Alipay, WeChat Pay, etc. For specific payment methods and operation guides
PRODUCTCERTIFICATES
The company’s honor certificate highlights the strength of the enterprise, enhances the brand image, enhances customer trust, helps market expansion, and promotes cooperation opportunities.
Credibility Enhancement
Company certificates directly reflect corporate credibility, significantly boosting the trust of customers and partners.
Market Expansion
Attract more potential customers and partners, and bring more business opportunities for enterprises.
Compliance Assurance
Companies can demonstrate compliance with industry standards and legal and regulatory requirements to reduce operational risk.
CONTACTUS
- +86 158 7179 3200
- info@fdiamond.cn
- No. 601, Block B, Optics Valley International Talent Port, No. 815 Gaoxin Avenue, Wuhan, Hubei
• Step PDC Cutter
Step-shaped PDC cutters are affixed to cutting equipment using bolt fixation rather than the traditional brazing method.
PRODUCTDESIGN

The innovative Step-shaped PDC cutter design revolutionizes cutter replacement with its bolt fixation system, abandoning traditional brazing methods. This forward-thinking approach enables swift and seamless swaps of worn-out cutters with new ones, significantly boosting operational efficiency. The cleverly engineered small steps at the bottom of these cutters provide a secure anchor point, allowing for robust bolt fastening to the equipment.

Excellent Wear Resistance

Customized Services

Good Thermal Stability

Outstanding Impact Resistance
PRODUCTSPECIFICATIONS
| Type | Diameter | Height | Diamond layer height | Step height | Step diameter | Diamond chamfer size |
| SCS0808 | 8.00mm | 8.00mm | 2.0mm | 1.5mm | 4mm | 0.40mm×45° |
| SCS1008 | 10.00mm | 8.00mm | 2.0mm | 1.5mm | 4mm | 0.40mm×45° |
| SCS1308 | 13.44mm | 8.00mm | 2.0mm | 1.5mm | 6mm | 0.40mm×45° |
| SCS1311 | 13.44mm | 11.00mm | 2.0mm | 3mm | 6mm | 0.40mm×45° |
| SCS1313 | 13.44mm | 13.20mm | 2.0mm | 5.2mm | 6mm | 0.40mm×45° |
OURADVANTAGES

These distinct advantages can significantly aid Field Diamond in distinguishing itself amidst the fiercely competitive market landscape, effectively bolstering its overall competitiveness and positioning it as a leading player in its industry.
- Leading Technology Innovation
- High Production Efficiency
- Optimized Cost Control
- Strict Quality Control
- Green and Environmentally Friendly Production
APPLICATIONAREAS
It is widely used in oil drilling, geological exploration, coal mine drilling rig, mechanical processing tools and other industries.
Natural gas &
Oil operation
Water well
building
Down-the-hole
hammer
Geological
exploration
PRODUCTIONPROCESS
From the preparation of raw materials to the final product, the entire production process reflects the advanced nature and professionalism of modern production.
FACTORYSHOWCASE
Advanced equipment, production processes.
High degree of equipment automation, excellent product quality.
Intelligent and efficient equipment, streamlined and smooth process.
Field Diamond help companies stand out in the fierce market competition.
325+
Complete Projects
750+
Innovative Solutions Deployed
15+
Certified Experts
1000+
Milestones Achieved in Development
SOMEFAQ
● PDC Cutter FAQ
PDC composite sheet is a composite material sintered by diamond micropowder and cemented carbide substrate under ultra-high pressure and high temperature conditions, which combines the high hardness and wear resistance of diamond and the strength and impact toughness of cemented carbide.
UsualPDC tools are widely used in oil drilling, geological exploration, mechanical processing, wood processing and other fields.
PDC tools have higher hardness, wear resistance and thermal stability, which can significantly improve the durability and processing quality of the tool, and have better economy.
The PDC composite sheet is made of natural or synthetic diamond powder and binder (including cobalt, nickel and other metals) sintered on the cemented carbide matrix at high temperature and pressure.
● Custom service and technical support FAQ
Yes, we offer customized services for PDC tools to meet the specific needs of different customers.
The delivery time for customized products depends on the specific customization content and production schedule. Generally, after receiving the customization request, we will assess it as soon as possible and provide an estimated delivery time.
We offer comprehensive technical support, including product selection consultation, installation guidance, troubleshooting, and resolution. Customers can contact us via phone, email, or online chat tools to obtain timely technical support.
● Production and processing of PDC tools FAQ
Our production process includes raw material preparation, mixing, sintering, grinding and polishing and other links, each link has undergone strict quality control to ensure stable and reliable product performance.
We use advanced production equipment and technology, high production efficiency, can meet the needs of large orders.
The processing process of PDC tool includes the cutting of PDC composite sheet, blade welding, blade sharpening and other steps, each link needs precise control to ensure tool performance.
We use advanced processing equipment and technology, while equipped with professional technical personnel for quality control, to ensure that the processing accuracy of PDC tools meet customer requirements.
● Order FAQ
You can order online through our official website, or you can contact our sales team directly for product information and help. For large purchases or customized needs, it is recommended to communicate in detail by email or phone, so that we can provide you with more accurate quotes and services.
Generally, standard products are shipped within 3-7 working days after order confirmation and payment. For customized or specially configured products, the shipping time may be slightly longer, subject to our production schedule and customer communication. We will notify you of the estimated shipping date in advance.
We support multiple payment methods, including but not limited to bank transfers, credit card payments (through third-party payment platforms), Alipay, WeChat Pay, etc. For specific payment methods and operation guides
PRODUCTCERTIFICATES
The company’s honor certificate highlights the strength of the enterprise, enhances the brand image, enhances customer trust, helps market expansion, and promotes cooperation opportunities.
Credibility Enhancement
Company certificates directly reflect corporate credibility, significantly boosting the trust of customers and partners.
Market Expansion
Attract more potential customers and partners, and bring more business opportunities for enterprises.
CONTACTUS

- +86 158 7179 3200
- info@fdiamond.cn
- No. 601, Block B, Optics Valley International Talent Port, No. 815 Gaoxin Avenue, Wuhan, Hubei
Submit your request to us
And we will contact you within 24 hours
kingpdc