Ridge Shaped PDC Cutter

Series: OGRS1308 / OGRS1313 / OGRS1613 / OGRS1913

This page focuses on kingpdc's documented OGRS configurations within the wider ridge shaped PDC cutter category. Four model records define diameter, height, diamond-layer height and chamfers. Conditional formation and drilling-system guidance explains where ridge geometry can enter a bit design and which variables still control field results. Drawings, formation data, operating conditions, quantity and destination make a sample or production quotation technically meaningful.

  • ModelsOGRS1308, OGRS1313, OGRS1613, OGRS1913
  • Diameter13.44-19.05 mm / 0.529-0.750 in
  • Overall Height8.00 or 13.20 mm / 0.315 or 0.520 in
  • Diamond Layer2.8 mm / 0.110 in
  • ApplicationSoft-to-medium-hard formations; oil and gas; geothermal
  • PlacementPrimary cutter; orientation and pocket geometry are drawing-controlled

Routine production lead time is 7-15 days after model, shape, quantity and customization requirements are fixed.

Which OGRS Size Fits Your Cutter Pocket?

The documented diameter and height establish the initial match; the approved drawing then governs pocket geometry, joining clearance, ridge orientation and tolerances.

ModelDiameterOverall heightDiamond layer
OGRS130813.44 mm / 0.529 in8.00 mm / 0.315 in2.8 mm / 0.110 in
OGRS131313.44 mm / 0.529 in13.20 mm / 0.520 in2.8 mm / 0.110 in
OGRS161315.88 mm / 0.625 in13.20 mm / 0.520 in2.8 mm / 0.110 in
OGRS191319.05 mm / 0.750 in13.20 mm / 0.520 in2.8 mm / 0.110 in

Selection conclusion: OGRS1308 matches a 13 mm-class pocket that requires the shorter body. OGRS1313, OGRS1613 and OGRS1913 share the 13.20 mm / 0.520 in body height at their documented diameters. The approved drawing remains the production authority.

When Should Ridge Geometry Enter The Bit Design?

The raised working face creates an early contact zone that can concentrate local loading and change chip flow compared with a flat face.

The official OGRS reference positions these cutters for primary-cutter duty in soft-to-medium-hard formations, including oil-and-gas and geothermal work. Independent engineering literature also associates ridge or stepped faces with changed cutting-force and vibration response under its stated test and simulation conditions.

Decision boundary: treat the ridge as one design variable, not a performance guarantee. Formation variability, cutter position, ridge direction, exposure, WOB, RPM, hydraulics and complete-bit dynamics determine the field result. Validate survival and wear with a sample or controlled bit trial.

What Makes A Ridge Cutter RFQ Buildable?

A usable quotation connects the requested geometry to the bit, formation, inspection and delivery plan.

Geometry and interfaceOGRS model or drawing, ridge orientation, pocket diameter and depth, joining method, exposure and chamfers
ApplicationBit type and position, formation description, abrasiveness/interbeds, WOB, RPM, hydraulics and known failure mode
VerificationSample quantity, dimensional report, lot traceability, test plan and customer-side field validation
Commercial basisOrder quantity, destination, delivery target, packaging, required documents and Incoterms location

Recommendation: a drawing and operating envelope paired with quantity and destination allows kingpdc to define either a standard sample route or a custom review.

Ridge Shaped PDC Cutter OGRS Specifications

The four documented OGRS configurations provide the nominal comparison, while the approved order drawing governs release tolerances and the pocket interface.

Product NameRidge Shaped PDC Cutter
ModelsOGRS1308, OGRS1313, OGRS1613, OGRS1913
Product CategoryNon-planar polycrystalline diamond compact cutter
Nominal SizesDiameter 13.44-19.05 mm (0.529-0.750 in); height 8.00-13.20 mm (0.315-0.520 in)
Size ToleranceNominal values shown; final tolerances follow the approved order drawing
Material CompositionPolycrystalline diamond working layer bonded to a cemented-tungsten-carbide substrate
Connection InterfaceCylindrical carbide substrate; pocket and joining clearance by approved bit drawing
Applicable StandardBuyer-approved drawing and inspection plan; ISO 9001 covers the management system, not cutter performance
Marking and TraceabilityModel, lot and drawing revision to be agreed in the purchase order and inspection record
Packaging UnitIndividually protected working faces; final pack quantity and labeling by order

Ridge Cutter Performance and Working Conditions

Documented dimensions are exact; formation and drilling behavior remain conditional on the selected cutter, bit layout and operating plan.

4 modelsDocumented OGRS configurations
13.44-19.05 mm0.529-0.750 in diameter range
2.8 mm0.110 in documented diamond-layer height
7-15 daysRoutine production window after order definition
Working MediumRock cutting in fixed-cutter drilling tools; documented range: soft-to-medium-hard formations, oil and gas, and geothermal wells
Temperature LimitsThermal suitability depends on cooling, exposure time and the selected PCD grade; the project operating envelope defines the accepted limit
Pressure and LoadAccepted WOB, RPM and impact exposure are defined at complete-bit level for the formation and cutter layout
Installation LimitsRidge orientation, primary-cutter position, exposure, pocket geometry, joining process and chip clearance are drawing-controlled

Ridge Shaped PDC Cutter MOQ, Price and Delivery

Commercial terms align the sample route, production quantity, budgetary starting reference, lead time, packing, payment and shipping basis.

  • Minimum Order QuantityThe OGRS model, material grade, quantity and inspection scope establish the order minimum
  • Sample PolicySamples and technical specifications can be supplied for customer or bit-manufacturer validation
  • Sample Lead TimeThe selected model, quantity and inspection requirements establish the sample schedule
  • Bulk Lead TimeRoutine production is 7-15 days; shape, quantity and customization can change it
  • Price and AvailabilityFrom USD 20.00 per piece, PreOrder; non-binding budgetary reference. The final quote is calculated from model, grade, quantity, inspection, packing and trade term.
  • PackagingThe order defines diamond-face protection, labels and pack quantity
  • Payment TermsThe formal quotation and purchase order define payment terms
  • Shipping SupportDHL, FedEx or SF under agreed logistics and insurance terms

Who Supplies and Supports the OGRS Range?

Wuhan Field Diamond supports application review, samples, configured cutter supply, inspection coordination and export logistics.

Field Diamond production and inspection areaField Diamond manufacturing facility

Wuhan Field Diamond Co., Ltd.

No. 601, Block B, Optics Valley International Talent Port, No. 815 Gaoxin Avenue, Wuhan, Hubei.

Supported activities include application-adapted PDC cutter supply, technical consultation, samples, custom chamfers, optional cobalt-removal service, inspection coordination and export shipping.

  • Samples can be supplied for customer or bit-manufacturer field validation.
  • Routine production lead time is 7-15 days after the order definition is fixed.
  • DHL, FedEx and SF logistics can be arranged under the agreed shipping basis.

Current and Historical Certification Evidence

The current ISO 9001 management-system certificate is separated from historical API drill-bit records to keep scope and validity clear.

Field Diamond certification record 1Field Diamond certification record 2Field Diamond certification record 3Field Diamond certification record 4Field Diamond certification record 5Field Diamond certification record 6
  • ISO 9001 Quality Management SystemGB/T 19001-2016 / ISO 9001:2015; certificate 46025Q0212R0S; issued February 7, 2025; valid through February 6, 2028 subject to surveillance. Scope: sales of superhard-material products, drilling tools and accessories.
  • API Monogram 7-1-1242Historical/expired record for PDC and roller-cone drill bits; effective date shown as August 19, 2022. Not a current cutter certification.
  • API Spec Q1 Q1-4970Historical/expired drill-bit registration; effective date shown as July 27, 2023. Not a current OGRS product approval.

Request a Ridge Shaped PDC Cutter Quote

  • Phone: +86 138 8687 9351
  • Email: info@fdiamond.cn
  • Address: No. 601, Block B, Optics Valley International Talent Port, No. 815 Gaoxin Avenue, Wuhan, Hubei

Your contact details are used only to respond to this product inquiry.