Our high-performance pdc drill bits for sale is designed with premium-grade polycrystalline diamond compact and reinforced body to provide extremely high rate of penetration and long footage life for oil, mine and geothermal drilling.
Composite sheet diameter:
8mm – 19mm optional
Applicable strata:
soft to medium hard strata with f≤ 12
Joint standard:
API standard screw thread


high-quality 13mm/16mm PDC cutting teeth are selected, the thermal stability is improved by 30%, the cutting edge sharpness can be maintained even in abrasive formation, and the total footage of a single drill bit is increased by more than 40% compared with ordinary models.

3-7 replaceable tungsten steel nozzles are configured, combined with the asymmetric chip removal groove design, so that the chip removal efficiency is increased by 25%, and the mud bag phenomenon of drill bit in clay layer operation is effectively prevented.

high-density diamond reinforcement column and hard alloy block are embedded in the diameter-keeping part, and the borehole tolerance is strictly controlled within ± 0.02mm, which greatly reduces the need for reaming and reduces the lateral vibration of the drilling tool.

The matrix drill bit is sintered with high content of tungsten carbide, which has strong erosion resistance and wear resistance, and can effectively protect the integrity of the blade under the environment of high flow rate drilling fluid.

the steel body drill bit is made of high-performance alloy steel. After five-axis CNC overall machining and surface hardening treatment, the toughness is extremely high, and it can withstand severe impact load without blade fracture.

through computer simulation analysis, the force balance teeth are distributed, so that the lateral force of the drill bit tends to zero when rotating at high speed, the drilling stability is improved by 35%, and the life of the drill bit and downhole power drilling tools is significantly prolonged.
| Parameter name | Technical Specifications / Detailed Description |
| Product Type | Matrix Body / Steel Body |
| Number of blades | 3, 4, 5, 6, 8 blades are optional. |
| Cutting tooth dimensions | 8mm, 10mm, 13mm, 16mm, 19mm |
| Formation hardness (Standard) | Soft to medium hard formations |
| Compressive strength | 10,000 – 25,000 PSI |
| Recommended RPM | 60 – 150 RPM (adjusted according to formation) |
| Interface type | 2-3/8″, 3-1/2″, 4-1/2″, 6-5/8″ API Reg/IF |
| Diameter-keeping materials | Sintered tungsten carbide + diamond reinforcing column |
Industry-leading wear resistance and cutting efficiency:
Compared with similar products, our pdc drill bits for sale adopts a new generation of controlled sintering technology, which improves the impact resistance of PDC sheets by 20%. Under the same pressure conditions, the penetration rate is 15%-20% higher than the industry standard on average, which can effectively shorten the drilling cycle.
Excellent stability and life performance:
This series of drills is optimized by fluid dynamics to ensure that the coolant can reach the center of the cutting edge. This not only reduces the risk of tooth collapse caused by high temperature, but also extends the service life of the drill bit in complex formations by about 30%, significantly reducing the comprehensive rental and replacement costs of the purchasing manager.


In view of the expensive standby cost caused by the easy wear of the drill bit in deep well operation, the high wear-resistant PDC composite sheet will increase the footage of a single drill bit by more than 50%.

By optimizing the balance design of the blade, the problem of early cracking failure of the cutting blade caused by the severe vibration of the drill bit in the soft and hard alternating rock layer is solved.

the use of enhanced heat dissipation runner and high thermal stability composite sheet, to solve the deep well operation due to poor heat dissipation caused by the softening of the composite sheet metal bond problem.

Suitable for drilling in straight, directional and horizontal sections of land and offshore oil and gas wells, reducing the cost of drilling per meter through high footage.

provide stable and efficient rock crushing capacity in CBM development, metal deposit survey and vent construction.

for large-diameter geothermal well drilling, to provide high-temperature, long-life cutting program, significantly shorten the delivery cycle of high-strength construction.

in bridge foundation pile drilling, trenchless horizontal directional drilling and other projects, to deal with complex formation changes and maintain efficient operations.

Product life expectancy and instructions for use:
At the recommended weight-on-bit and rotation speed, the footage life of a single drill bit in geologically matched formations can usually reach 3000-6000 meters. Before use, please check the threads and apply special thread oil, and ensure that the bottom of the well is clean. It is strictly forbidden to forcibly smash the bottom rock.

Pre-sales and after-sales service:
Provide professional formation characteristics analysis services to assist the purchasing manager in selecting the most matching number of blades and tooth arrangement. The quality tracking of “No.1 1 file” is implemented for the products. The after-sales team responds to technical consultation 24 hours a day and provides professional repair suggestions and evaluation reports for worn drill bits.

The steel drill bit has good impact resistance and toughness, and is suitable for shallow wells requiring large chip removal and fast drilling. The matrix drill bit has strong erosion resistance and is more suitable for deep wells, high abrasive formations and long-life operation requirements.
PDC bits perform best in soft to medium hard formations. For extremely hard or abrasive hard rock, we recommend that you use our reinforced small diameter cloth tooth models designed specifically for hard formations.
The drill bits we produce fully conform to API specifications, including 2-3/8 “API Reg, 3-1/2” API Reg, 4-1/2 “API Reg, etc., which can be directly adapted to various drill pipes.
Our drill bit adopts a large flow channel design and polished blade surface, combined with the turbulence generated by the adjustable nozzle, which can effectively scour debris and prevent mud adhesion.
19mm and other large diameter cutting teeth have higher footage in soft formations; while 13mm or smaller cutting teeth are more stable in harder or heterogeneous formations.
We provide bit loss assessment. If the body structure is complete, only individual composite sheet wear, can guide or assist in the replacement of composite sheet, in order to save the cost of secondary procurement.
Our high-performance pdc drill bits for sale is designed with premium-grade polycrystalline diamond compact and reinforced body to provide extremely high rate of penetration and long footage life for oil, mine and geothermal drilling.

Composite sheet diameter:
8mm – 19mm optional
Applicable strata:
soft to medium hard strata with f≤ 12
Joint standard:
API standard screw thread

high-quality 13mm/16mm PDC cutting teeth are selected, the thermal stability is improved by 30%, the cutting edge sharpness can be maintained even in abrasive formation, and the total footage of a single drill bit is increased by more than 40% compared with ordinary models.

3-7 replaceable tungsten steel nozzles are configured, combined with the asymmetric chip removal groove design, so that the chip removal efficiency is increased by 25%, and the mud bag phenomenon of drill bit in clay layer operation is effectively prevented.

high-density diamond reinforcement column and hard alloy block are embedded in the diameter-keeping part, and the borehole tolerance is strictly controlled within ± 0.02mm, which greatly reduces the need for reaming and reduces the lateral vibration of the drilling tool.

The matrix drill bit is sintered with high content of tungsten carbide, which has strong erosion resistance and wear resistance, and can effectively protect the integrity of the blade under the environment of high flow rate drilling fluid.

the steel body drill bit is made of high-performance alloy steel. After five-axis CNC overall machining and surface hardening treatment, the toughness is extremely high, and it can withstand severe impact load without blade fracture.

through computer simulation analysis, the force balance teeth are distributed, so that the lateral force of the drill bit tends to zero when rotating at high speed, the drilling stability is improved by 35%, and the life of the drill bit and downhole power drilling tools is significantly prolonged.
| Parameter name | Technical Specifications / Detailed Description |
| Product Type | Matrix Body / Steel Body |
| Number of blades | 3, 4, 5, 6, 8 blades are optional. |
| Cutting tooth dimensions | 8mm, 10mm, 13mm, 16mm, 19mm |
| Formation hardness (Standard) | Soft to medium hard formations |
| Compressive strength | 10,000 – 25,000 PSI |
| Recommended RPM | 60 – 150 RPM (adjusted according to formation) |
| Interface type | 2-3/8″, 3-1/2″, 4-1/2″, 6-5/8″ API Reg/IF |
| Diameter-keeping materials | Sintered tungsten carbide + diamond reinforcing column |
Industry-leading wear resistance and cutting efficiency:
Compared with similar products, our pdc drill bits for sale adopts a new generation of controlled sintering technology, which improves the impact resistance of PDC sheets by 20%. Under the same pressure conditions, the penetration rate is 15%-20% higher than the industry standard on average, which can effectively shorten the drilling cycle.
Excellent stability and life performance:
This series of drills is optimized by fluid dynamics to ensure that the coolant can reach the center of the cutting edge. This not only reduces the risk of tooth collapse caused by high temperature, but also extends the service life of the drill bit in complex formations by about 30%, significantly reducing the comprehensive rental and replacement costs of the purchasing manager.


In view of the expensive standby cost caused by the easy wear of the drill bit in deep well operation, the high wear-resistant PDC composite sheet will increase the footage of a single drill bit by more than 50%.

By optimizing the balance design of the blade, the problem of early cracking failure of the cutting blade caused by the severe vibration of the drill bit in the soft and hard alternating rock layer is solved.

the use of enhanced heat dissipation runner and high thermal stability composite sheet, to solve the deep well operation due to poor heat dissipation caused by the softening of the composite sheet metal bond problem.

Suitable for drilling in straight, directional and horizontal sections of land and offshore oil and gas wells, reducing the cost of drilling per meter through high footage.

provide stable and efficient rock crushing capacity in CBM development, metal deposit survey and vent construction.

for large-diameter geothermal well drilling, to provide high-temperature, long-life cutting program, significantly shorten the delivery cycle of high-strength construction.

in bridge foundation pile drilling, trenchless horizontal directional drilling and other projects, to deal with complex formation changes and maintain efficient operations.

Product life expectancy and instructions for use:
At the recommended weight-on-bit and rotation speed, the footage life of a single drill bit in geologically matched formations can usually reach 3000-6000 meters. Before use, please check the threads and apply special thread oil, and ensure that the bottom of the well is clean. It is strictly forbidden to forcibly smash the bottom rock.

Pre-sales and after-sales service:
Provide professional formation characteristics analysis services to assist the purchasing manager in selecting the most matching number of blades and tooth arrangement. The quality tracking of “No.1 1 file” is implemented for the products. The after-sales team responds to technical consultation 24 hours a day and provides professional repair suggestions and evaluation reports for worn drill bits.
The steel drill bit has good impact resistance and toughness, and is suitable for shallow wells requiring large chip removal and fast drilling. The matrix drill bit has strong erosion resistance and is more suitable for deep wells, high abrasive formations and long-life operation requirements.
PDC bits perform best in soft to medium hard formations. For extremely hard or abrasive hard rock, we recommend that you use our reinforced small diameter cloth tooth models designed specifically for hard formations.
The drill bits we produce fully conform to API specifications, including 2-3/8 “API Reg, 3-1/2” API Reg, 4-1/2 “API Reg, etc., which can be directly adapted to various drill pipes.
Our drill bit adopts a large flow channel design and polished blade surface, combined with the turbulence generated by the adjustable nozzle, which can effectively scour debris and prevent mud adhesion.
19mm and other large diameter cutting teeth have higher footage in soft formations; while 13mm or smaller cutting teeth are more stable in harder or heterogeneous formations.
We provide bit loss assessment. If the body structure is complete, only individual composite sheet wear, can guide or assist in the replacement of composite sheet, in order to save the cost of secondary procurement.