Flat PDC Cutters are manufactured through a unique high-temperature and high-pressure process using customized raw materials, complemented by technologies like finite element analysis, temperature, and pressure measurement, ensuring excellent performance. Structurally, they consist of a polycrystalline diamond layer (for wear resistance and impact toughness) and a tungsten carbide substrate (for support and stability).

Depending on the application market and drill bit position, Flat PDC Cutters are available in various types: economic (TRA), wear-resistant (TD), impact-resistant (TC), and comprehensive (TAH), catering to diverse formations and drilling conditions.

Flat PDC Cutter(images 10)

Using a polycrystalline diamond layer, Flat PDC Cutters have extremely high hardness.

Flat PDC Cutter(images 11)

Customized according to specific needs, including shape, wear resistance, impact resistance, etc.

Flat PDC Cutter(images 12)

It is not easy to deform or fail due to thermal expansion, thus ensuring the continuity and safety of drilling operations.

Flat PDC Cutter(images 13)

With strong shock and vibration, thereby extending the service life.

undefined

PRODUCTSPECIFICATIONS

TypeDiameterHeightDiamond layer heightDiamond chamfer sizeCarbide chamfer size
OGF08088.00/8.20mm8.00mm2.0/2.5/ 3.0mm0.40mm×45°0.76mm×45°
OGF08138.00/8.20mm13.20mm2.0/2.5/ 3.0mm0.40mm×45°0.76mm×45°
OGF100810.00mm8.00mm2.0/2.5/ 3.0mm0.40mm×45°0.76mm×45°
OGF101310.00mm13.20mm2.0/2.5/ 3.0mm0.40mm×45°0.76mm×45°
OGF130813.44mm8.00mm2.0/2.5/ 3.0mm0.40mm×45°0.76mm×45°
OGF131313.44mm13.20mm2.0/2.5/ 3.0mm0.40mm×45°0.76mm×45°
OGF160815.88/16.10mm8.00mm2.0/2.5/ 3.0mm0.40mm×45°0.76mm×45°
OGF161315.88/16.10mm13.20mm2.0/2.5/ 3.0mm0.40mm×45°0.76mm×45°
OGF190819.05mm8.00mm2.0/2.5/ 3.0mm0.40mm×45°0.76mm×45°
OGF191319.05mm13.20mm2.0/2.5/ 3.0mm0.40mm×45°0.76mm×45°

OURADVANTAGES

These distinct advantages can significantly aid Field Diamond in distinguishing itself amidst the fiercely competitive market landscape, effectively bolstering its overall competitiveness and positioning it as a leading player in its industry.

  • Leading Technology Innovation
  • High Production Efficiency
  • Optimized Cost Control
  • Strict Quality Control
  • Green and Environmentally Friendly Production

16K+

Customer

Satisfied

Campaigns

Client Satisfaction

Years Experiences

Certified Experts

APPLICATIONAREAS

Natural gas & Oiloperation ——

Down-the-hole hammer ——

Water well building ——

Geological 

exploration ——

With the strength and impact resistance of cemented carbide, it is an ideal material for manufacturing wear-resistant tools such as cutting tools and drills, and has a wide range of applications in oil drilling, geological exploration, coal mine drills, mechanical processing tools and other industries.

With its exceptional strength and impact resistance, cemented carbide is an ideal material for manufacturing wear-resistant tools, widely applied in oil drilling, geological exploration, mining, machinery, and more. 

PRODUCTIONPROCESS

The process begins with the preparation of raw materials, which are screened and inspected to ensure their quality meets production requirements. The raw material then enters the HTHP (high temperature and high pressure) synthesis stage, where it is converted into synthetic blocks through specific process conditions.

Next, the synthetic block goes through a series of treatment steps, including machining, grinding, etc., to further improve its properties and shape. In this process, advanced technologies such as electric discharge machining (EDM) and shaping are also used to ensure the accuracy and surface quality of the product.

Finally, after fine processing such as laser treatment, the individual parts are assembled together to form the final product. The entire production process is rigorous and efficient, reflecting the advanced nature and professionalism of modern production.

Flat PDC Cutter(images 15)
Flat PDC Cutter(images 16)
Flat PDC Cutter(images 17)
Flat PDC Cutter(images 18)
Flat PDC Cutter(images 19)
Flat PDC Cutter(images 20)
Flat PDC Cutter(images 21)
Flat PDC Cutter(images 22)

FACTORYSHOWCASE

SOMEFAQ

01 What are PDC composite products?

PDC composite sheet is a composite material sintered by diamond micropowder and cemented carbide substrate under ultra-high pressure and high temperature conditions, which combines the high hardness and wear resistance of diamond and the strength and impact toughness of cemented carbide.

02 What are the main application areas of PDC tools?

UsualPDC tools are widely used in oil drilling, geological exploration, mechanical processing, wood processing and other fields.

03 What are the advantages of PDC tools over traditional tools?

PDC tools have higher hardness, wear resistance and thermal stability, which can significantly improve the durability and processing quality of the tool, and have better economy.

04 How are PDC composites made?

The PDC composite sheet is made of natural or synthetic diamond powder and binder (including cobalt, nickel and other metals) sintered on the cemented carbide matrix at high temperature and pressure.

01 Do you offer product customization services?

Yes, we offer customized services for PDC tools to meet the specific needs of different customers.

02 What is the delivery time for customized products?

The delivery time for customized products depends on the specific customization content and production schedule. Generally, after receiving the customization request, we will assess it as soon as possible and provide an estimated delivery time.

03 What technical support do you offer?

We offer comprehensive technical support, including product selection consultation, installation guidance, troubleshooting, and resolution. Customers can contact us via phone, email, or online chat tools to obtain timely technical support.

01 What is your production process for PDC composite products?

Our production process includes raw material preparation, mixing, sintering, grinding and polishing and other links, each link has undergone strict quality control to ensure stable and reliable product performance.

02 What is the production efficiency of PDC composite products?

We use advanced production equipment and technology, high production efficiency, can meet the needs of large orders.

03 What steps does the PDC tool process include?

The processing process of PDC tool includes the cutting of PDC composite sheet, blade welding, blade sharpening and other steps, each link needs precise control to ensure tool performance.

04 How does your company guarantee the machining accuracy of PDC composite slices?

We use advanced processing equipment and technology, while equipped with professional technical personnel for quality control, to ensure that the processing accuracy of PDC tools meet customer requirements.

01 How can I place an order for your products?

You can order online through our official website, or you can contact our sales team directly for product information and help. For large purchases or customized needs, it is recommended to communicate in detail by email or phone, so that we can provide you with more accurate quotes and services.

02 How long does it usually take to ship after order confirmation?

Generally, standard products are shipped within 3-7 working days after order confirmation and payment. For customized or specially configured products, the shipping time may be slightly longer, subject to our production schedule and customer communication. We will notify you of the estimated shipping date in advance.

03 What payment methods do you accept?

We support multiple payment methods, including but not limited to bank transfers, credit card payments (through third-party payment platforms), Alipay, WeChat Pay, etc. For specific payment methods and operation guides

PRODUCTCERTIFICATES

Flat PDC Cutter(images 23)
Flat PDC Cutter(images 24)
Flat PDC Cutter(images 25)
Flat PDC Cutter(images 26)
Flat PDC Cutter(images 27)
Flat PDC Cutter(images 28)
Flat PDC Cutter(images 29)

Credibility Enhancement

Flat PDC Cutter(images 30)

Market Expansion

Flat PDC Cutter(images 31)

Compliance Assurance

CONTACTUS

*
*

Please select your requirement type

16131313oil&gas drillingwell drilling
Submitting!
Submitted successfully!
Submission failed! Please try again later!
Email format error!
Phone format error!
  • +86 158 7179 3200
  • info@fdiamond.cn
  • No. 601, Block B, Optics Valley International Talent Port, No. 815 Gaoxin Avenue, Wuhan, Hubei
Flat PDC Cutter(images 32)

• Flat PDC Cutter

The most common PDC cutters shape on drill bits is the diamond end face, known for its high flatness and suitability for rock cutting operations.

PRODUCTDESIGN

Flat PDC Cutter(images 33)

Flat PDC Cutters are manufactured through a unique high-temperature and high-pressure process using customized raw materials, complemented by technologies like finite element analysis, temperature, and pressure measurement, ensuring excellent performance. Structurally, they consist of a polycrystalline diamond layer (for wear resistance and impact toughness) and a tungsten carbide substrate (for support and stability).

Flat PDC Cutter(images 34)

Excellent Wear Resistance

Flat PDC Cutter(images 35)

Customized Services

Flat PDC Cutter(images 36)

Good Thermal Stability

Flat PDC Cutter(images 37)

Outstanding Impact Resistance

PRODUCTSPECIFICATIONS

TypeDiameterHeightDiamond layer heightDiamond chamfer sizeCarbide chamfer size
OGF08088.00/8.20mm8.00mm2.0/2.5/ 3.0mm0.40mm×45°0.76mm×45°
OGF08138.00/8.20mm13.20mm2.0/2.5/ 3.0mm0.40mm×45°0.76mm×45°
OGF100810.00mm8.00mm2.0/2.5/ 3.0mm0.40mm×45°0.76mm×45°
OGF101310.00mm13.20mm2.0/2.5/ 3.0mm0.40mm×45°0.76mm×45°
OGF130813.44mm8.00mm2.0/2.5/ 3.0mm0.40mm×45°0.76mm×45°
OGF131313.44mm13.20mm2.0/2.5/ 3.0mm0.40mm×45°0.76mm×45°
OGF160815.88/16.10mm8.00mm2.0/2.5/ 3.0mm0.40mm×45°0.76mm×45°
OGF161315.88/16.10mm13.20mm2.0/2.5/ 3.0mm0.40mm×45°0.76mm×45°
OGF190819.05mm8.00mm2.0/2.5/ 3.0mm0.40mm×45°0.76mm×45°
OGF191319.05mm13.20mm2.0/2.5/ 3.0mm0.40mm×45°0.76mm×45°

OURADVANTAGES

Flat PDC Cutter(images 38)

These distinct advantages can significantly aid Field Diamond in distinguishing itself amidst the fiercely competitive market landscape, effectively bolstering its overall competitiveness and positioning it as a leading player in its industry.

  • Leading Technology Innovation
  • High Production Efficiency
  • Optimized Cost Control
  • Strict Quality Control
  • Green and Environmentally Friendly Production

APPLICATIONAREAS

It is widely used in oil drilling, geological exploration, coal mine drilling rig, mechanical processing tools and other industries.

Natural gas & 

Oil operation

Water well

building

Down-the-hole

hammer

Geological 

exploration

PRODUCTIONPROCESS

From the preparation of raw materials to the final product, the entire production process reflects the advanced nature and professionalism of modern production.

Flat PDC Cutter(images 39)
Flat PDC Cutter(images 40)
Flat PDC Cutter(images 41)
Flat PDC Cutter(images 42)
Flat PDC Cutter(images 43)
Flat PDC Cutter(images 44)
Flat PDC Cutter(images 45)
Flat PDC Cutter(images 46)

FACTORYSHOWCASE

Field Diamond help companies stand out in the fierce market competition.

SOMEFAQ

01 What are PDC composite products?

PDC composite sheet is a composite material sintered by diamond micropowder and cemented carbide substrate under ultra-high pressure and high temperature conditions, which combines the high hardness and wear resistance of diamond and the strength and impact toughness of cemented carbide.

02 What are the main application areas of PDC tools?

UsualPDC tools are widely used in oil drilling, geological exploration, mechanical processing, wood processing and other fields.

03 What are the advantages of PDC tools over traditional tools?

PDC tools have higher hardness, wear resistance and thermal stability, which can significantly improve the durability and processing quality of the tool, and have better economy.

04 How are PDC composites made?

The PDC composite sheet is made of natural or synthetic diamond powder and binder (including cobalt, nickel and other metals) sintered on the cemented carbide matrix at high temperature and pressure.

01 Do you offer product customization services?

Yes, we offer customized services for PDC tools to meet the specific needs of different customers.

02 What is the delivery time for customized products?

The delivery time for customized products depends on the specific customization content and production schedule. Generally, after receiving the customization request, we will assess it as soon as possible and provide an estimated delivery time.

03 What technical support do you offer?

We offer comprehensive technical support, including product selection consultation, installation guidance, troubleshooting, and resolution. Customers can contact us via phone, email, or online chat tools to obtain timely technical support.

01 What is your production process for PDC composite products?

Our production process includes raw material preparation, mixing, sintering, grinding and polishing and other links, each link has undergone strict quality control to ensure stable and reliable product performance.

02 What is the production efficiency of PDC composite products?

We use advanced production equipment and technology, high production efficiency, can meet the needs of large orders.

03 What steps does the PDC tool process include?

The processing process of PDC tool includes the cutting of PDC composite sheet, blade welding, blade sharpening and other steps, each link needs precise control to ensure tool performance.

04 How does your company guarantee the machining accuracy of PDC composite slices?

We use advanced processing equipment and technology, while equipped with professional technical personnel for quality control, to ensure that the processing accuracy of PDC tools meet customer requirements.

01 How can I place an order for your products?

You can order online through our official website, or you can contact our sales team directly for product information and help. For large purchases or customized needs, it is recommended to communicate in detail by email or phone, so that we can provide you with more accurate quotes and services.

02 How long does it usually take to ship after order confirmation?

Generally, standard products are shipped within 3-7 working days after order confirmation and payment. For customized or specially configured products, the shipping time may be slightly longer, subject to our production schedule and customer communication. We will notify you of the estimated shipping date in advance.

03 What payment methods do you accept?

We support multiple payment methods, including but not limited to bank transfers, credit card payments (through third-party payment platforms), Alipay, WeChat Pay, etc. For specific payment methods and operation guides

PRODUCTCERTIFICATES

Flat PDC Cutter(images 47)

Credibility Enhancement

Flat PDC Cutter(images 48)

Market Expansion

Flat PDC Cutter(images 49)
Flat PDC Cutter(images 50)
Flat PDC Cutter(images 51)
Flat PDC Cutter(images 52)
Flat PDC Cutter(images 53)

CONTACTUS

Flat PDC Cutter(images 54)
  • +86 158 7179 3200
  • info@fdiamond.cn
  • No. 601, Block B, Optics Valley International Talent Port, No. 815 Gaoxin Avenue, Wuhan, Hubei

Submit your request to us

And we will contact you within 24 hours

*
*

Please select your requirement type

16131313oil&gas drillingwell drilling
Submitting!
Submitted successfully!
Submission failed! Please try again later!
Email format error!
Phone format error!