product search

Step PDC Cutter(images 1)
Step PDC Cutter(images 2)

Step PDC Cutter

Step PDC cutter features a step structure for staged rock breaking, reduced contact area to minimize frictional heat, and enhanced stability for reliable performance.

  • Application:Pavement Cutting,Stone Cutting
  • Placement:Primary Cutter
  • Size:0808 1008 1308 1311 1313

PRODUCTDESIGN

The innovative Step-shaped PDC cutter design revolutionizes cutter replacement with its bolt fixation system, abandoning traditional brazing methods. This forward-thinking approach enables swift and seamless swaps of worn-out cutters with new ones, significantly boosting operational efficiency. The cleverly engineered small steps at the bottom of these cutters provide a secure anchor point, allowing for robust bolt fastening to the equipment.

This clever design tweak translates to reduced downtime, minimized labor costs, and increased productivity. By simplifying the replacement process, operators can quickly get back to drilling, ensuring uninterrupted progress and maximizing their drilling potential.

Step PDC Cutter(images 3)

Using a polycrystalline diamond layer, Step PDC Cutter have extremely high hardness.

Step PDC Cutter(images 4)

Customized according to specific needs, including shape, wear resistance, impact resistance, etc.

Step PDC Cutter(images 5)

It is not easy to deform or fail due to thermal expansion, thus ensuring the continuity and safety of drilling operations.

Step PDC Cutter(images 6)

With strong shock and vibration, thereby extending the service life.

Step PDC Cutter(images 7)
  • Step structure enables staged rock breaking
  • Reduced contact area reduces frictional heat
  • Enhanced stability
undefined

PRODUCTSPECIFICATIONS

TypeDiameterHeightDiamond layer heightStep heightStep diameterDiamond chamfer size
SCS08088.00mm8.00mm2.0mm1.5mm4mm0.40mm×45°
SCS100810.00mm8.00mm2.0mm1.5mm4mm0.40mm×45°
SCS130813.44mm8.00mm2.0mm1.5mm6mm0.40mm×45°
SCS131113.44mm11.00mm2.0mm3mm6mm0.40mm×45°
SCS131313.44mm13.20mm2.0mm5.2mm6mm0.40mm×45°

OURADVANTAGES

These distinct advantages can significantly aid Field Diamond in distinguishing itself amidst the fiercely competitive market landscape, effectively bolstering its overall competitiveness and positioning it as a leading player in its industry.

  • Leading Technology Innovation
  • High Production Efficiency
  • Optimized Cost Control
  • Strict Quality Control
  • Green and Environmentally Friendly Production

16K+

Customer

Satisfied

Campaigns

Client Satisfaction

Years Experiences

Certified Experts

APPLICATIONAREAS

Natural gas & Oiloperation ——

Down-the-hole hammer ——

Water well building ——

Geological 

exploration ——

With the strength and impact resistance of cemented carbide, it is an ideal material for manufacturing wear-resistant tools such as cutting tools and drills, and has a wide range of applications in oil drilling, geological exploration, coal mine drills, mechanical processing tools and other industries.

With its exceptional strength and impact resistance, cemented carbide is an ideal material for manufacturing wear-resistant tools, widely applied in oil drilling, geological exploration, mining, machinery, and more. 

FACTORYSHOWCASE

PRODUCTCERTIFICATES

Step PDC Cutter(images 9)
Step PDC Cutter(images 10)
Step PDC Cutter(images 11)
Step PDC Cutter(images 12)
Step PDC Cutter(images 13)
Step PDC Cutter(images 14)
Step PDC Cutter(images 15)

Credibility Enhancement

Step PDC Cutter(images 16)

Market Expansion

Step PDC Cutter(images 17)

Compliance Assurance

CONTACTUS

*
*

Please select your requirement type

16131313oil&gas drillingwell drilling
Submitting!
Submitted successfully!
Submission failed! Please try again later!
Email format error!
Phone format error!
  • +86 158 7179 3200
  • [email protected]
  • No. 601, Block B, Optics Valley International Talent Port, No. 815 Gaoxin Avenue, Wuhan, Hubei
Step PDC Cutter(images 18)

• Step PDC Cutter

Step-shaped PDC cutters are affixed to cutting equipment using bolt fixation rather than the traditional brazing method.

PRODUCTDESIGN

Step PDC Cutter(images 19)

The innovative Step-shaped PDC cutter design revolutionizes cutter replacement with its bolt fixation system, abandoning traditional brazing methods. This forward-thinking approach enables swift and seamless swaps of worn-out cutters with new ones, significantly boosting operational efficiency. The cleverly engineered small steps at the bottom of these cutters provide a secure anchor point, allowing for robust bolt fastening to the equipment.

Step PDC Cutter(images 20)

Excellent Wear Resistance

Step PDC Cutter(images 21)

Customized Services

Step PDC Cutter(images 22)

Good Thermal Stability

Step PDC Cutter(images 23)

Outstanding Impact Resistance

PRODUCTSPECIFICATIONS

TypeDiameterHeightDiamond layer heightStep heightStep diameterDiamond chamfer size
SCS08088.00mm8.00mm2.0mm1.5mm4mm0.40mm×45°
SCS100810.00mm8.00mm2.0mm1.5mm4mm0.40mm×45°
SCS130813.44mm8.00mm2.0mm1.5mm6mm0.40mm×45°
SCS131113.44mm11.00mm2.0mm3mm6mm0.40mm×45°
SCS131313.44mm13.20mm2.0mm5.2mm6mm0.40mm×45°

OURADVANTAGES

Step PDC Cutter(images 24)

These distinct advantages can significantly aid Field Diamond in distinguishing itself amidst the fiercely competitive market landscape, effectively bolstering its overall competitiveness and positioning it as a leading player in its industry.

  • Leading Technology Innovation
  • High Production Efficiency
  • Optimized Cost Control
  • Strict Quality Control
  • Green and Environmentally Friendly Production

APPLICATIONAREAS

It is widely used in oil drilling, geological exploration, coal mine drilling rig, mechanical processing tools and other industries.

Natural gas & 

Oil operation

Water well

building

Down-the-hole

hammer

Geological 

exploration

PRODUCTIONPROCESS

From the preparation of raw materials to the final product, the entire production process reflects the advanced nature and professionalism of modern production.

Step PDC Cutter(images 25)
Step PDC Cutter(images 26)
Step PDC Cutter(images 27)
Step PDC Cutter(images 28)
Step PDC Cutter(images 29)
Step PDC Cutter(images 30)
Step PDC Cutter(images 31)
Step PDC Cutter(images 32)

FACTORYSHOWCASE

Field Diamond help companies stand out in the fierce market competition.

SOMEFAQ

01 What are PDC composite products?

PDC composite sheet is a composite material sintered by diamond micropowder and cemented carbide substrate under ultra-high pressure and high temperature conditions, which combines the high hardness and wear resistance of diamond and the strength and impact toughness of cemented carbide.

02 What are the main application areas of PDC tools?

UsualPDC tools are widely used in oil drilling, geological exploration, mechanical processing, wood processing and other fields.

03 What are the advantages of PDC tools over traditional tools?

PDC tools have higher hardness, wear resistance and thermal stability, which can significantly improve the durability and processing quality of the tool, and have better economy.

04 How are PDC composites made?

The PDC composite sheet is made of natural or synthetic diamond powder and binder (including cobalt, nickel and other metals) sintered on the cemented carbide matrix at high temperature and pressure.

01 Do you offer product customization services?

Yes, we offer customized services for PDC tools to meet the specific needs of different customers.

02 What is the delivery time for customized products?

The delivery time for customized products depends on the specific customization content and production schedule. Generally, after receiving the customization request, we will assess it as soon as possible and provide an estimated delivery time.

03 What technical support do you offer?

We offer comprehensive technical support, including product selection consultation, installation guidance, troubleshooting, and resolution. Customers can contact us via phone, email, or online chat tools to obtain timely technical support.

01 What is your production process for PDC composite products?

Our production process includes raw material preparation, mixing, sintering, grinding and polishing and other links, each link has undergone strict quality control to ensure stable and reliable product performance.

02 What is the production efficiency of PDC composite products?

We use advanced production equipment and technology, high production efficiency, can meet the needs of large orders.

03 What steps does the PDC tool process include?

The processing process of PDC tool includes the cutting of PDC composite sheet, blade welding, blade sharpening and other steps, each link needs precise control to ensure tool performance.

04 How does your company guarantee the machining accuracy of PDC composite slices?

We use advanced processing equipment and technology, while equipped with professional technical personnel for quality control, to ensure that the processing accuracy of PDC tools meet customer requirements.

01 How can I place an order for your products?

You can order online through our official website, or you can contact our sales team directly for product information and help. For large purchases or customized needs, it is recommended to communicate in detail by email or phone, so that we can provide you with more accurate quotes and services.

02 How long does it usually take to ship after order confirmation?

Generally, standard products are shipped within 3-7 working days after order confirmation and payment. For customized or specially configured products, the shipping time may be slightly longer, subject to our production schedule and customer communication. We will notify you of the estimated shipping date in advance.

03 What payment methods do you accept?

We support multiple payment methods, including but not limited to bank transfers, credit card payments (through third-party payment platforms), Alipay, WeChat Pay, etc. For specific payment methods and operation guides

PRODUCTCERTIFICATES

Step PDC Cutter(images 33)

Credibility Enhancement

Step PDC Cutter(images 34)

Market Expansion

Step PDC Cutter(images 35)
Step PDC Cutter(images 36)
Step PDC Cutter(images 37)
Step PDC Cutter(images 38)
Step PDC Cutter(images 39)

CONTACTUS

Step PDC Cutter(images 40)
  • +86 158 7179 3200
  • [email protected]
  • No. 601, Block B, Optics Valley International Talent Port, No. 815 Gaoxin Avenue, Wuhan, Hubei

Submit your request to us

And we will contact you within 24 hours

*
*

Please select your requirement type

16131313oil&gas drillingwell drilling
Submitting!
Submitted successfully!
Submission failed! Please try again later!
Email format error!
Phone format error!

*
*
*
Submitting…
Submitted successfully!
Submission failed!
Invalid email address!
Invalid phone number!

Free Sample Available!

Send Us a Message

*
*
*
Submitting…
Submitted successfully!
Submission failed!
Invalid email address!
Invalid phone number!

This will close in 0 seconds