Flat PDC Cutter
Flat PDC Cutter offers a flat structure for uniform force, exceptional wear resistance for longer service life, and versatile, cost-effective performance.
- Application:Oil and gas, Water Wells, Coal Mining
- Placement:Primary Cutter、Gauge Cutter
- Size:0808 1013 1108 1305 1308 1313 1608 1613 1616 1908 1913 1916
PRODUCTDESIGN
Flat PDC Cutters are manufactured through a unique high-temperature and high-pressure process using customized raw materials, complemented by technologies like finite element analysis, temperature, and pressure measurement, ensuring excellent performance. Structurally, they consist of a polycrystalline diamond layer (for wear resistance and impact toughness) and a tungsten carbide substrate (for support and stability).
Depending on the application market and drill bit position, Flat PDC Cutters are available in various types: economic (TRA), wear-resistant (TD), impact-resistant (TC), and comprehensive (TAH), catering to diverse formations and drilling conditions.

Excellent Wear Resistance
Using a polycrystalline diamond layer, Flat PDC Cutters have extremely high hardness.

Customized Services
Customized according to specific needs, including shape, wear resistance, impact resistance, etc.

Preeminent Thermal Stability
It is not easy to deform or fail due to thermal expansion, thus ensuring the continuity and safety of drilling operations.

Outstanding Impact Resistance
With strong shock and vibration, thereby extending the service life.
PRODUCTSPECIFICATIONS
| Type | Diameter | Height | Diamond layer height | Diamond chamfer size | Carbide chamfer size |
| OGF0808 | 8.00/8.20mm | 8.00mm | 2.0/2.5/ 3.0mm | 0.40mm×45° | 0.76mm×45° |
| OGF0813 | 8.00/8.20mm | 13.20mm | 2.0/2.5/ 3.0mm | 0.40mm×45° | 0.76mm×45° |
| OGF1008 | 10.00mm | 8.00mm | 2.0/2.5/ 3.0mm | 0.40mm×45° | 0.76mm×45° |
| OGF1013 | 10.00mm | 13.20mm | 2.0/2.5/ 3.0mm | 0.40mm×45° | 0.76mm×45° |
| OGF1308 | 13.44mm | 8.00mm | 2.0/2.5/ 3.0mm | 0.40mm×45° | 0.76mm×45° |
| OGF1313 | 13.44mm | 13.20mm | 2.0/2.5/ 3.0mm | 0.40mm×45° | 0.76mm×45° |
| OGF1608 | 15.88/16.10mm | 8.00mm | 2.0/2.5/ 3.0mm | 0.40mm×45° | 0.76mm×45° |
| OGF1613 | 15.88/16.10mm | 13.20mm | 2.0/2.5/ 3.0mm | 0.40mm×45° | 0.76mm×45° |
| OGF1908 | 19.05mm | 8.00mm | 2.0/2.5/ 3.0mm | 0.40mm×45° | 0.76mm×45° |
| OGF1913 | 19.05mm | 13.20mm | 2.0/2.5/ 3.0mm | 0.40mm×45° | 0.76mm×45° |
OURADVANTAGES
These distinct advantages can significantly aid Field Diamond in distinguishing itself amidst the fiercely competitive market landscape, effectively bolstering its overall competitiveness and positioning it as a leading player in its industry.
- Leading Technology Innovation
- High Production Efficiency
- Optimized Cost Control
- Strict Quality Control
- Green and Environmentally Friendly Production
16K+
Customer
Satisfied
500+
Campaigns
98%
Client Satisfaction
7+
Years Experiences
15+
Certified Experts
APPLICATIONAREAS
Natural gas & Oiloperation ——
Down-the-hole hammer ——
Water well building ——
Geological
exploration ——
• All Projects
With the strength and impact resistance of cemented carbide, it is an ideal material for manufacturing wear-resistant tools such as cutting tools and drills, and has a wide range of applications in oil drilling, geological exploration, coal mine drills, mechanical processing tools and other industries.
With its exceptional strength and impact resistance, cemented carbide is an ideal material for manufacturing wear-resistant tools, widely applied in oil drilling, geological exploration, mining, machinery, and more.
FACTORYSHOWCASE
Field Diamond help companies stand out in the fierce market competition.
Our factory integrates advanced equipment, exquisite technology and efficient management, and ensures excellent product quality with strict quality control system. We have a professional research and development team, continuous innovation, to meet the needs of diversified markets. Large-scale production to reduce costs, to provide cost-effective quality products, to win customer trust and praise.
325+
Complete Projects
15+
Certified Experts
750+
Innovative Solutions Deployed
1000+
Milestones Achieved in Development
Scale production
Advanced equipment, production processes.
High-effect
High degree of equipment automation, excellent product quality and stability.
Lean manufacturing
Intelligent and efficient equipment, streamlined and smooth process.
PRODUCTCERTIFICATES
The company’s honor certificate highlights the strength of the enterprise, enhances the brand image, enhances customer trust, helps market expansion, and promotes cooperation opportunities.
Credibility Enhancement
Company certificates directly reflect corporate credibility, significantly boosting the trust of customers and partners.
Market Expansion
Attract more potential customers and partners, and bring more business opportunities for enterprises.
Compliance Assurance
Companies can demonstrate compliance with industry standards and legal and regulatory requirements to reduce operational risk.
CONTACTUS
- +86 158 7179 3200
- [email protected]
- No. 1306-13F, C23 Software New Town, Huacheng Avenue, Wuhan, 430076, China
—— relational production ——
related products
• Flat PDC Cutter
The most common PDC cutters shape on drill bits is the diamond end face, known for its high flatness and suitability for rock cutting operations.
PRODUCTDESIGN

Flat PDC Cutters are manufactured through a unique high-temperature and high-pressure process using customized raw materials, complemented by technologies like finite element analysis, temperature, and pressure measurement, ensuring excellent performance. Structurally, they consist of a polycrystalline diamond layer (for wear resistance and impact toughness) and a tungsten carbide substrate (for support and stability).

Excellent Wear Resistance

Customized Services

Good Thermal Stability

Outstanding Impact Resistance
PRODUCTSPECIFICATIONS
| Type | Diameter | Height | Diamond layer height | Diamond chamfer size | Carbide chamfer size |
| OGF0808 | 8.00/8.20mm | 8.00mm | 2.0/2.5/ 3.0mm | 0.40mm×45° | 0.76mm×45° |
| OGF0813 | 8.00/8.20mm | 13.20mm | 2.0/2.5/ 3.0mm | 0.40mm×45° | 0.76mm×45° |
| OGF1008 | 10.00mm | 8.00mm | 2.0/2.5/ 3.0mm | 0.40mm×45° | 0.76mm×45° |
| OGF1013 | 10.00mm | 13.20mm | 2.0/2.5/ 3.0mm | 0.40mm×45° | 0.76mm×45° |
| OGF1308 | 13.44mm | 8.00mm | 2.0/2.5/ 3.0mm | 0.40mm×45° | 0.76mm×45° |
| OGF1313 | 13.44mm | 13.20mm | 2.0/2.5/ 3.0mm | 0.40mm×45° | 0.76mm×45° |
| OGF1608 | 15.88/16.10mm | 8.00mm | 2.0/2.5/ 3.0mm | 0.40mm×45° | 0.76mm×45° |
| OGF1613 | 15.88/16.10mm | 13.20mm | 2.0/2.5/ 3.0mm | 0.40mm×45° | 0.76mm×45° |
| OGF1908 | 19.05mm | 8.00mm | 2.0/2.5/ 3.0mm | 0.40mm×45° | 0.76mm×45° |
| OGF1913 | 19.05mm | 13.20mm | 2.0/2.5/ 3.0mm | 0.40mm×45° | 0.76mm×45° |
OURADVANTAGES

These distinct advantages can significantly aid Field Diamond in distinguishing itself amidst the fiercely competitive market landscape, effectively bolstering its overall competitiveness and positioning it as a leading player in its industry.
- Leading Technology Innovation
- High Production Efficiency
- Optimized Cost Control
- Strict Quality Control
- Green and Environmentally Friendly Production
APPLICATIONAREAS
It is widely used in oil drilling, geological exploration, coal mine drilling rig, mechanical processing tools and other industries.
Natural gas &
Oil operation
Water well
building
Down-the-hole
hammer
Geological
exploration
PRODUCTIONPROCESS
From the preparation of raw materials to the final product, the entire production process reflects the advanced nature and professionalism of modern production.
FACTORYSHOWCASE
Advanced equipment, production processes.
High degree of equipment automation, excellent product quality.
Intelligent and efficient equipment, streamlined and smooth process.
Field Diamond help companies stand out in the fierce market competition.
325+
Complete Projects
750+
Innovative Solutions Deployed
15+
Certified Experts
1000+
Milestones Achieved in Development
SOMEFAQ
● PDC Cutter FAQ
PDC composite sheet is a composite material sintered by diamond micropowder and cemented carbide substrate under ultra-high pressure and high temperature conditions, which combines the high hardness and wear resistance of diamond and the strength and impact toughness of cemented carbide.
UsualPDC tools are widely used in oil drilling, geological exploration, mechanical processing, wood processing and other fields.
PDC tools have higher hardness, wear resistance and thermal stability, which can significantly improve the durability and processing quality of the tool, and have better economy.
The PDC composite sheet is made of natural or synthetic diamond powder and binder (including cobalt, nickel and other metals) sintered on the cemented carbide matrix at high temperature and pressure.
● Custom service and technical support FAQ
Yes, we offer customized services for PDC tools to meet the specific needs of different customers.
The delivery time for customized products depends on the specific customization content and production schedule. Generally, after receiving the customization request, we will assess it as soon as possible and provide an estimated delivery time.
We offer comprehensive technical support, including product selection consultation, installation guidance, troubleshooting, and resolution. Customers can contact us via phone, email, or online chat tools to obtain timely technical support.
● Production and processing of PDC tools FAQ
Our production process includes raw material preparation, mixing, sintering, grinding and polishing and other links, each link has undergone strict quality control to ensure stable and reliable product performance.
We use advanced production equipment and technology, high production efficiency, can meet the needs of large orders.
The processing process of PDC tool includes the cutting of PDC composite sheet, blade welding, blade sharpening and other steps, each link needs precise control to ensure tool performance.
We use advanced processing equipment and technology, while equipped with professional technical personnel for quality control, to ensure that the processing accuracy of PDC tools meet customer requirements.
● Order FAQ
You can order online through our official website, or you can contact our sales team directly for product information and help. For large purchases or customized needs, it is recommended to communicate in detail by email or phone, so that we can provide you with more accurate quotes and services.
Generally, standard products are shipped within 3-7 working days after order confirmation and payment. For customized or specially configured products, the shipping time may be slightly longer, subject to our production schedule and customer communication. We will notify you of the estimated shipping date in advance.
We support multiple payment methods, including but not limited to bank transfers, credit card payments (through third-party payment platforms), Alipay, WeChat Pay, etc. For specific payment methods and operation guides
PRODUCTCERTIFICATES
The company’s honor certificate highlights the strength of the enterprise, enhances the brand image, enhances customer trust, helps market expansion, and promotes cooperation opportunities.
Credibility Enhancement
Company certificates directly reflect corporate credibility, significantly boosting the trust of customers and partners.
Market Expansion
Attract more potential customers and partners, and bring more business opportunities for enterprises.
CONTACTUS

- +86 158 7179 3200
- [email protected]
- No. 1306-13F, C23 Software New Town, Huacheng Avenue, Wuhan, 430076, China
Submit your request to us
And we will contact you within 24 hours
kingpdc